The quality of the plating, is directly proportional to the quality of the material being plated. The criteria that need to be considered during the injection process is as follows:
The material should be kept at 80-100 °C for a minimum of 2 hours to prevent splatter.
Mold release agents (Silicone) should never be sprayed onto the mold surface.
If possible, parts should not be handled by hand when they come out of the injection mold; operators should wear gloves.
To ensure the durability of the plating, Natural ABS suitable for plating should be used. For the appropriate raw material, please contact our company.